HS-1064P Unsaturated Polyester Resin for Flame Retardant FRP Lighting Panels

HS-1064P resin is a kind of unsaturated polyester resin specially used for making flame retardant light transmitting FRP lighting boards, which can reach the requirement of first class flame retardant with good infiltration of glass fibre, good light transmittance and weathering, excellent mechanical strength and flame retardant property. It is suitable for machine or hand-laid moulding of light-emitting boards (tiles).
This product complies with the EU ROHS directive on lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls (PBBs) and polybrominated diphenyl ethers (PBDEs).
Availability:
  • HS-1064P

  • Huake

Product Description

HS-1064P  Unsaturated Polyester Resin
Characteristics and main uses:
HS-1064P resin is a kind of unsaturated polyester resin specially used for making flame retardant light transmitting FRP lighting boards, which can reach the requirement of first class flame retardant with good infiltration of glass fibre, good light transmittance and weathering, excellent mechanical strength and flame retardant property. It is suitable for machine or hand-laid moulding of light-emitting boards (tiles).
This product complies with the EU ROHS directive on lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls (PBBs) and polybrominated diphenyl ethers (PBDEs).

 Liquid resin technical indicators:
Item Unit Specification Test Method
Appearance --- Purple-red transparent liquid GB/T 8237.6.1.1
Viscosity 25ºC , cp 180-260 GB/T 7193.4.1
SPI-GT min. 0.5-2.0 GB/T 7193.4.4
SPI-CT min. 2.0-4.0 GB/T 7193.4.4
SPI-PET ºC 185-220 GB/T 7193.4.4
Solid Ccontent % 60-70 GB/T 2895
Note: When testing SPI curing properties, the curing system is: accelerator KC: 2%; curing agent M-50: 1.2%.


Physical properties of Casting(for reference only):

 
Item Unit Measured Value Test Method
Tensile Strength MPa 55 GB/T 2568
Bending Strength MPa 90 GB/T 2570
Elongation at Break % 3.5 GB/T 2568
Heat Distortion Temperature ºC 60 GB/T 1634
Oxygen Index % 30 GB/T 3854
Note: 1) The casting system sample method is implemented according to GB/T 8237.
Curing system: accelerator (0.6% Co-Naph): 2%, curing agent (AKZO M-50): 2%;
(2) Post-curing treatment of casting body: room temperature×24 hours+60ºC×3 hours+100ºC×2 hours.


Precautions:

Transportation should be in accordance with the provisions of the State Council's 'Regulations on the Safe Management of Dangerous Chemicals', Chapter V, Transportation and Handling of Dangerous Chemical Substances. The product should be stored in a cool place under 25ºC, avoid fire, isolate heat source, and keep it sealed to prevent moisture intrusion and volatilisation of monomer. Shelf life is 3 months when stored under 25ºC.
 


Previous: 
Next: 

Related News

content is empty!

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap