+86-19802502739
 marketing@huakepolymers.com
Products
Home » Markets » Sanitary Wares » Low Styrene Emission Unsaturated Polyester Resin for FRP Reinforcement Layer HS-1102GH (LS)

loading

Share to:
facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
kakao sharing button
snapchat sharing button
sharethis sharing button

Low Styrene Emission Unsaturated Polyester Resin for FRP Reinforcement Layer HS-1102GH (LS)

HS-1102GH(LS) is a low styrene emission unsaturated polyester resin designed for acrylic bonding layers. It features with pre-acceleration, thixotropy. It bonds well with acrylic sheets, with a low shrinkage rate with the finished product. It is suitable for FRP reinforcement layer for the hand lay-up/spray-molded acrylic sanitary ware.
Availability:
  • HS-1102GH(LS)

  • HUAKE

Product Description

HS-1102GH (LS) Unsaturated Polyester Resin


Principal Properties & Application: 


HS-1102GH(LS) is a low styrene emission unsaturated polyester resin designed for acrylic bonding layers. It features with pre-acceleration, thixotropy. It bonds well with acrylic sheets, with a low shrinkage rate with the finished product. It is suitable for FRP reinforcement layer for the hand lay-up/spray-molded acrylic sanitary ware.


Specifications of liquid resin:


Properties

Value

Test Method

Appearance

Cyan turbid liquid

GB/T 8237.6.1.1

Viscosity(25℃,cP)

80-100

GB/T 7193.4.1

*Gel-time(25℃,min.)

10.0-40.0

GB/T 7193.4.6

Thixotropic Index

2.5-3.5

HK-F-TM-03

*Curing system in GT test: Hardener AKZO M-50: 1%.

HS-1102GH (LS) Unsaturated Polyester Resin
Application
Previous: 
Next: 

Subscribe To Our Newsletter

Leave your email address to get the latest product information from our company at any time.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-19802502739
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap