Unsaturated Polyester Resin HS-1010B

HS-1010B is a kind of unsaturated polyester resin which is used in the production of FRP lighting plate. The FRP made of it has good wettability, mechanical strength , transparency, and anti-aging performance when exposed to the ultraviolet. HS-1010B is suitable for both machine and hand lay-up method.
Availability:
  • HS-1010B

  • HUAKE

Product Description

Principal Properties & Application:

HS-1010B is a kind of unsaturated polyester resin which is used in the production of FRP lighting plate. The FRP made of it has good wettability, mechanical strength , transparency, and anti-aging performance when exposed to the ultraviolet. HS-1010B is suitable for both machine and hand lay-up method.


Specifications of liquid resin:

Item

Standard Requirements

Test Method

Remark

Appearance

Light yellow

transparent liquid

HK-F-TM-00


Colour

≦50

HK-F-TM-01

Hazen

Viscosity(25℃,cP)

120-190

HK-F-TM-03

November to March

180-250

HK-F-TM-03

April to May, September to October

250-350

HK-F-TM-03

June to August

*Gel time(25℃,min)

9.0-13.0

HK-F-TM-10


*Curing system in GT test:Accelerator KC: 2%;hardener AKZO M-50: 2%.


Physical properties of casting(for reference only):

Item

Unit

Test Value

Test Method

Tensile strength

MPa

65

GB/T 2568

Tensile modulus

MPa

3550

GB/T 2568

Breaking elongation

%

1.9

GB/T 2568

Flexural strength

MPa

112

GB/T 2570

Flexural modulus

MPa

3650

GB/T 2570

Impact strength

KJ/m2

10.5

GB/T 2571

HDT

℃

78

GB/T 1634

Hardness (Barcol 934-1)

--

46

GB/T 3854

Note:1) Curing System: 0.6%Co-Naph 1% ; MEKP 1%;

2) Post curing:RT×24hrs +60℃×3hrs+100℃×2hrs.


Application

|Application:

HS-1010B is suitable for FRP lighting plate.


Lighting Panel (2)_副本

Lighting Panel

Lighting Panel (3)_副本

Lighting Panel

Lighting Panel (3)

Lighting Panel



HS-1010B TDS
Previous: 
Next: 

Related News

content is empty!

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap