DP-1102D Unsaturated Polyester Resin for FRP Sheet And Pipes

The DP-1102D series is a medium-viscosity, ortho-phthalic type unsaturated polyester resin with good mechanical strength. It is suitable for making the structural layer of fiber-wound (sandwiched) FRP pipes, as well as hand lay-up and pultrusion molded FRP products. Among them, DP-1102D-Y contains wax, and DP-1102D-N does not contain wax.
Availability:
  • DP-1102D

  • HUAKE

Product Description

Principal Properties:

The DP-1102D series is a medium-viscosity, ortho-phthalic type unsaturated polyester resin with good mechanical strength. It is suitable for making the structural layer of fiber-wound (sandwiched) FRP pipes, as well as hand lay-up and pultrusion molded FRP products. Among them, DP-1102D-Y contains wax, and DP-1102D-N does not contain wax.


Specifications of Liquid Resin:

Item

Unit

Indicator

Test Method

Appearance

--

Light yellow transparent liquid

GB/T 8237.6.1.1

Viscosity

25℃, cP

300-450

GB/T 7193.4.1

Gel Time

min

10.0-20.0

GB/T 7193.4.6

Solid Content

%

60.0-68.0

GB/T 7193.4.3

*Curing system in GT test: curing agent: AKZO M-50 2%; Promoter: 0.6% Co-Naph, 2%.


Physical Properties of Casting(for reference only):

Item

Unit

Measured Value

Test Method

Heat Distortion Temperature

℃

68

GB/T 1634

Tensile Strength

MPa

70

GB/T 2568

Tensile Modulus

MPa

3021

GB/T 2568

Elongation at Break

%

3.92

GB/T 2568

Flexural Strength

MPa

115

GB/T 2570

Flexural Modulus

MPa

3540

GB/T 2570

Impact Strength

KJ/M2

12.9

GB/T 2571

Barcol Hardness

Barcol

41

GB/T 3854

Note:

1)The casting system sample method is executed according to GB/T 8237.

2)Curing System: Hardener AKZO M-50: 1.5%; 0.6% Co-Naph 2%.

3) Post curing: RT × 24 h + 60℃×3h+100℃×2h.


Application

|Application:

The DP-1102D is suitable for making the structural layer of fiber-wound (sandwiched) FRP pipes, as well as hand lay-up and pultrusion molded FRP products


不透明板材

 Lighting Panel

半透明板材_副本

Lighting Panel

半透明采光板_副本

Lighting Panel



DP-1102D TDS
Previous: 
Next: 

Related News

content is empty!

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18014995084
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap