HS-1013S Unsaturated Polyester Resin

HS-1013S is an unsaturated polyester resin specifically designed for making flame-retardant lighting panels. It has good light transmittance, mechanical strength, flame retardancy, and good weather resistance and yellowing resistance. It is suitable for both mechanized and hand lay-up processes.
Availability:
  • HS-1013S

  • HUAKE

Product Description

Principal Properties & Application:

HS-1013S is an unsaturated polyester resin specifically designed for making flame-retardant lighting panels. It has good light transmittance, mechanical strength, flame retardancy, and good weather resistance and yellowing resistance. It is suitable for both mechanized and hand lay-up processes.


Technical Specifications of Liquid Resin:

Item

Unit

Indicator

Test Method

Appearance

---

Light yellow transparent liquid

GB/T 8237.6.1.1

Viscosity

25℃, cp

180-260

GB/T 7193.4.1

SPI-GT

min

0.8-2.0

HK-D-DB001

SPI-CT

min

2.8-4.5

HK-D-DB001

SPI-PET

℃

180-210

HK-D-DB001

Color Code

Harzen

≤60

GB/T 605

Curing system in SPI test: Accelerator KC: 2% Hardener M-50: 1.2%;


Cast Physical properties(for reference only):

Item

Unit

Measured Value

Test Method

Tensile Strength

MPa

60

GB/T 2568

Bending Strength

MPa

108

GB/T 2570

Elongation at Break

%

3.0

GB/T 2568

Heat Distortion Temp

℃

70

GB/T 1634

Oxygen Index

%

26

GB/T 3854

Note:

1) The casting is made according to GB/T8237;

2) Accelerator (0.6% Co-Naph): 2%; Curing agent (AKZO M-50): 2%;

3) The post-curing conditions: RT×24hrs + 60℃×3hrs+100℃×2hrs.


Application

|Application:

HS-1013S is designed for making flame-retardant lighting panels.


Lighting Panel (2)_副本

Lighting Panel

Lighting Panel (3)_副本

Lighting Panel

Lighting Panel (3)

Lighting Panel



HS-1013S TDS
Previous: 
Next: 

Related News

content is empty!

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18014995084
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap