DP-1060H Flame-Retardant Resin for Lighting Fiberglass Sheet

DP-1060H resin is specially designed for making flame-retardant translucent fiberglass panels, meeting Class 1 flame retardancy requirements. It has good light transmission, mechanical strength, and flame retardancy, with excellent fiberglass wet-out properties.
Availability:
  • DP-1060H

  • HUAKE

Product Description

Principal Properties & Application:

Application: DP-1060H resin is specially designed for making flame-retardant translucent fiberglass panels, meeting Class 1 flame retardancy requirements. It has good light transmission, mechanical strength, and flame retardancy, with excellent fiberglass wet-out properties.

Suitability: Suitable for mechanized or hand lay-up forming of lighting panels (tiles).

Compliance: This product complies with the EU ROHS directive concerning lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls, and polybrominated diphenyl ethers content standards.


Technical Specifications of Liquid Resin:

Item

Unit

Indicator

Test Method

Appearance

---

Light yellow transparent liquid

GB/T 8237.6.1.1

Viscosity

25°C, cp

180-260

GB/T 7193.4.1

25°C GT

25°C, min

10-30

GB/T 7193.4.6

SPI-GT

min

1.0-2.0

HK-D-DB001

SPI-CT

min

2.6-4.0

HK-D-DB001

SPI-PET

°C

190-220

HK-D-DB001

Acid Value

mgKOH/g

15.0-25.0

GB/T 2895

Color Number

Harzen

≤ 60

GB/T 605

Curing system in SPI test: Accelerator KC: 2% Hardener M-50: 1.2%;


Cast Physical Properties(for reference only):

Item

Unit

Measured Value

Test Method

Tensile Strength

MPa

50

GB/T 2568

Flexural Strength

MPa

90

GB/T 2570

Elongation at Break

%

3.7

GB/T 2568

Heat Distortion Temp

°C

60

GB/T 1634

Oxygen Index

%

30

GB/T 3854

Note:

1) The casting is made according to GB/T8237;

2) Accelerator (0.6% Co-Naph): 2%; Curing agent (AKZO M-50): 2%;

3) The post-curing conditions: RT×24hrs+60℃×3hrs+100℃×2hrs.


Application

|Application:

DP-1060H is suitable for mechanized or hand lay-up forming of lighting panels (tiles).


D58134693(1)(1)

 Lighting Panel

D1288157_副本

Lighting Panel

Lighting Panel (3)_副本

Lighting Panel



DP-1060H TDS
Previous: 
Next: 

Related News

content is empty!

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18014995084
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap