+86-18648932615
 marketing@huakepolymers.com
Products
Home » Markets » Building & Construction » HS-1125 Orthophthalic Type Unsaturated Polyester Resin for SMC And BMC Products

loading

Share to:
facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
kakao sharing button
snapchat sharing button
sharethis sharing button

HS-1125 Orthophthalic Type Unsaturated Polyester Resin for SMC And BMC Products

HS-1125 is an Orthophthalic type unsaturated polyester resin, with high reactivity, medium viscosity and good thickening stability. Its products have good water resistance and toughness, as
well as excellent comprehensive mechanical properties. It is used in the production of low-pressure insulation parts, water tank panels, and other SMC/BMC products.
Availability:
  • HS-1125

  • HUAKE

Product Description

HS-1125 Unsaturated Polyester Resin

Principal Properties & Application: 

HS-1125 is an Orthophthalic type unsaturated polyester resin, with high reactivity, medium viscosity and good thickening stability. Its products have good water resistance and toughness, as well as excellent comprehensive mechanical properties. It is used in the production of low-pressure insulation parts, water tank panels, and other SMC/BMC products.


Specifications of liquid resin:

Item Unit Standard Requirements Test Method
Appearance --- Light yellow slightly turbid liquid GB/T 8237.6.1.1
Viscosity 25℃,mPa.s 1200-1400 GB/T 7193.4.1
SPI-GT min 6.0-8.0 HK-D-DB001
SPI-CT min 7.0-10.0 HK-D-DB001
SPI-PET ℃ 220-250 HK-D-DB001
Acidvalue mgKOH/g 19.0-25.0 GB/T 2895
Solid Content % 62.0-65.0 GB/T 7193.4.3
Water Content % <0.1 HK-D-DB007
Color Number(Hazen) --- ≤100 HK-D-DB036

Curing system in SPI test: Hardener AKZO CH-50: 2%.

Technical Data Sheet
Application
Previous: 
Next: 

Related News

content is empty!

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap