HS-1125 Orthophthalic Type Unsaturated Polyester Resin for SMC and BMC Products

Ko te HS-1125 he momo Orthophthalic polyester resin hamanga, me te hohenga teitei, te pokey reo me te pai o te whakapumautanga. Ko ona hua he pai te parenga wai me te uaua, me
nga taonga miihini tino pai. Kei te whakamahia i roto i te hanga o nga waahanga whakaheke-iti, nga panui tank wai, me etahi atu hua SMC / BMC.
Wāteatanga:
  • HS-1125

  • HUAKE

Whakaahuatanga Hua

HS-1125 Resin Polyester Kore Hanga

Ngā Āhuatanga Matua me te Taupānga: 

Ko te HS-1125 he momo Orthophthalic polyester resin hamanga, me te hohenga teitei, te pokey reo me te pai o te whakapumautanga. Ko ona hua he pai te parenga wai me te uaua, me nga taonga miihini tino pai. Kei te whakamahia i roto i te hanga o nga waahanga whakaheke-iti, nga panui tank wai, me etahi atu hua SMC / BMC.


Nga korero mo te kapia wai:

Tūemi Waeine Nga Whakaritenga Paerewa Tikanga Whakamatau
Te ahua --- He kowhai marama he wai kerekere GB/T 8237.6.1.1
Poneke 25℃,mPa.s 1200-1400 GB/T 7193.4.1
SPI-GT min 6.0-8.0 HK-D-DB001
SPI-CT min 7.0-10.0 HK-D-DB001
SPI-PET 220-250 HK-D-DB001
Uara Waikawa mgKOH/g 19.0-25.0 GB/T 2895
Ihirangi Mārō % 62.0-65.0 GB/T 7193.4.3
Ihirangi wai % <0.1 HK-D-DB007
Tau Tae(Hazen) --- ≤100 HK-D-DB036

Pūnaha whakaora i roto i te whakamatautau SPI: Hardener AKZO CH-50: 2%.

Pepa Raraunga Hangarau
Taupānga
Tōmua: 
Panuku: 

Nga korero e pa ana

he putua nga ihirangi!

Ohauru ki ta maatau Panui

Waiho to wahitau imeera ki te tiki i nga korero hua hou mai i ta maatau kamupene i nga wa katoa.
Ko Changzhou Huake polymer Co., Ltd. he tohungatanga ki te R&D, te whakaputa me te hoko o nga momo hua penei i te kapia polyester, te kapia vinyl me etahi atu.

NGA LINKO Tere

NGA HUA

WHAKAARO

  +86- 19802502739
  marketing@huakepolymers.com
  No.602, Te Tai Tokerau Yulong Road,
Takiwa Xinbei, Changzhou City,
Jiangsu Province, Haina.
Mana pupuri © 2024 Changzhou Huake polymer Co., Ltd. Katoa nga mana pupuri. Tautokona e leadong.com     Mahere pae