Resin Polyester Hakare mo te Taonga Puku DP-1102T(LS)

Ko te DP-1102T(LS) he kapia polyester hamanga iti o te styrene i hangaia mo nga papa herenga kiriaku. He iti te viscosity, i mua i te whakatere, te thixotropy, me te pai o te mahi. He iti te pāmahana tihi exothermic whakaora, a ka pai te hono ki nga pepa kiriaku, me te iti o te reiti whakaheke ki te hua kua oti. He pai mo te paparanga whakakaha FRP mo te taputapu horoi kiriaku-a-ringa.
Wāteatanga:
  • DP-1102T(LS)

  • HUAKE

Whakaahuatanga Hua

DP-1102T(LS) Resin Polyester Haanga


  • Ngā Āhuatanga Matua:


Ko te DP-1102T(LS) he kapia polyester hamanga iti o te styrene i hangaia mo nga papa herenga kiriaku. He iti te viscosity, i mua i te whakatere, te thixotropy, me te pai o te mahi. He iti te pāmahana tihi exothermic whakaora, a ka pai te hono ki nga pepa kiriaku, me te iti o te reiti whakaheke ki te hua kua oti. He pai mo te paparanga whakakaha FRP mo te taputapu horoi kiriaku-a-ringa.



  • Nga korero mo te kapia wai:


Āhuatanga

Uara

Tikanga Whakamatau

Te ahua

Wai Pokarekare

GB/T 8237.6.1.1

Viscosity(25℃,cP)

80-100

GB/T 7193.4.1

*Wa-wa (25 ℃, min)

10.0-40.0

GB/T 7193.4.6

Taurangi Thixotropic

2.0-3.5

GB/T 7193.4.1



*Pūnaha whakaora i roto i te whakamātautau GT: Hardener AKZO M-50: 1%.


DP-1102T(LS) TDS
Taupānga
Tōmua: 
Panuku: 

Changzhou Huake Polymer Co., Ltd.

I whakapau kaha a Huake ki te whakarato ki nga kaihoko nga hua o te kounga teitei me nga otinga matawhānui i roto i te mara o nga rauemi hiato me nga taapiri na roto i nga mahi hangarau.
Ko Changzhou Huake polymer Co., Ltd. he tohungatanga ki te R&D, te whakaputa me te hoko o nga momo hua penei i te kapia polyester, te kapia vinyl me etahi atu.

NGA LINKO Tere

NGA HUA

WHAKAARO

  +86-19802503183
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Mana pupuri © 2024 Changzhou Huake polymer Co., Ltd. Katoa nga mana pupuri. Tautokona e leadong.com     Mahere pae