Resin Polyester Unsaturated HS-1520 mo nga Hua SMC BMC

Ko te Hs-1520 he momo NPGl polyester kapia mo te SMC / BMC. He nui te tauhohenga, he iti te pokey, he pai te tae me nga ahuatanga whakakaha. He papatahi te mata o te hua, he kanapa teitei, he pai te aukati wai me te wera wera, te kaha o te miihini me te pai o te mahi hiko. E pa ana ki nga waahanga hiko, nga waahanga ahumahi, nga waahanga parukore, nga waahanga waka me etahi atu mara.
Wāteatanga:
  • HS-1520

  • HUAKE

Whakaahuatanga Hua

HS-1520 Resin Polyester Hangakore

Ngā Āhuatanga Matua me te Taupānga: 

Ko te HS-1520 he momo NPGl polyester kapia mo te SMC/BMC. He nui te tauhohenga, he iti te pokey, he pai te tae me nga ahuatanga whakakaha. He papatahi te mata o te hua, he kanapa teitei, he pai te aukati wai me te wera wera, te kaha o te miihini me te pai o te mahi hiko. E pa ana ki nga waahanga hiko, nga waahanga ahumahi, nga waahanga parukore, nga waahanga waka me etahi atu mara.


Nga korero mo te kapia wai:

Tūemi Waeine Nga Whakaritenga Paerewa Tikanga Whakamatau
Te ahua --- He kowhai marama he wai kerekere GB/T 8237.6.1.1
Poneke 25℃,mPa.s 600-800 GB/T 7193.4.1
SPI-GT min 6.0-8.0 HK-D-DB001
SPI-CT min 7.0-10.0 HK-D-DB001
SPI-PET 240-260 HK-D-DB001
Uara Waikawa mgKOH/g 12.5-15.5 GB/T 2895
Ihirangi % 59.0-63.0 GB/T 7193.4.3
Ihi wai % ≤0.08 HK-D-DB007
Waehere Tae --- ≤35 HK-D-DB036

SPI:2% BPO whakapiri.

Pepa Raraunga Hangarau
Taupānga
Tōmua: 
Panuku: 

Nga korero e pa ana

he putua nga ihirangi!

Ohauru ki ta maatau Panui

Waiho to wahitau imeera ki te tiki i nga korero hua hou mai i ta maatau kamupene i nga wa katoa.
Ko Changzhou Huake polymer Co., Ltd. he tohungatanga ki te R&D, te whakaputa me te hoko o nga momo hua penei i te kapia polyester haunga, te kapia vinyl me etahi atu.

NGA LINKO Tere

NGA HUA

WHAKAARO

  +86- 19802502739
  marketing@huakepolymers.com
  No.602, Te Tai Tokerau Yulong Road,
Takiwa Xinbei, Changzhou City,
Jiangsu Province, Haina.
Mana pupuri © 2024 Changzhou Huake polymer Co., Ltd. Katoa nga mana pupuri. Tautokona e leadong.com     Mahere pae