Unsaturated Polyester Resin HS-1520 for SMC BMC Products

Hs-1520 is a NPGl type unsaturated polyester resin for SMC / BMC. It has high reactivity, low viscosity, good coloring and thickening properties. The surface of the product is flat, with high gloss, excellent water resistance and heat resistance, high mechanical strength and good electrical performance. It is applicable to electrical parts, industrial parts, sanitary parts, vehicle parts and other fields.
Availability:
  • HS-1520

  • HUAKE

Product Description

HS-1520 Unsaturated Polyester Resin

Principal Properties & Application: 

HS-1520 is a NPGl type unsaturated polyester resin for SMC/BMC. It has high reactivity, low viscosity, good coloring and thickening properties. The surface of the product is flat, with high gloss, excellent water resistance and heat resistance, high mechanical strength and good electrical performance. It is applicable to electrical parts, industrial parts, sanitary parts, vehicle parts and other fields.


Specifications of liquid resin:

Item Unit Standard Requirements Test Method
Appearance --- Light yellow slightly turbid liquid GB/T 8237.6.1.1
Viscosity 25℃,mPa.s 600-800 GB/T 7193.4.1
SPI-GT min 6.0-8.0 HK-D-DB001
SPI-CT min 7.0-10.0 HK-D-DB001
SPI-PET ℃ 240-260 HK-D-DB001
Acidvalue mgKOH/g 12.5-15.5 GB/T 2895
Solidcontent % 59.0-63.0 GB/T 7193.4.3
Watercontent % ≤0.08 HK-D-DB007
Colorcode --- ≤35 HK-D-DB036

SPI:2% BPO paste.

Technical Data Sheet
Application
Previous: 
Next: 

Related News

content is empty!

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18014995084
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap