| Wāteatanga: | |
|---|---|
DP-1102D
HUAKE
Ngā Āhuatanga Matua:
Ko te raupapa DP-1102D he reo-potaka, momo ortho-phthalic momo polyester korehapu me te kaha miihini pai. He pai mo te hanga i te paparanga hanganga o nga putorino FRP kua werohia te muka (sandwiched), tae atu ki nga hua FRP hanga-a-ringa me te pultrusion. I roto ia ratou, kei roto i te DP-1102D-Y te wax, kaore he wax i te DP-1102D-N.
Ko nga korero mo te wai Resin:
Tūemi |
Waeine |
Tohutohu |
Tikanga Whakamatau |
Te ahua |
-- |
Te wai marama kowhai marama |
GB/T 8237.6.1.1 |
Poneke |
25℃, cP |
300-450 |
GB/T 7193.4.1 |
Waa Gel |
min |
10.0-20.0 |
GB/T 7193.4.6 |
Ihirangi Mārō |
% |
60.0-68.0 |
GB/T 7193.4.3 |
*Pūnaha whakaora i roto i te whakamātautau GT: māngai whakaora: AKZO M-50 2%; Kaiwhakatairanga: 0.6% Co-Naph, 2%.
Nga Tikanga tinana -a- o te C asting(mo te tohutoro anake):
Tūemi |
Waeine |
Uara ine |
Tikanga Whakamatau |
Te Wera Pawera |
℃ |
68 |
GB/T 1634 |
Te Kaha Toka |
MPa |
70 |
GB/T 2568 |
Kōwae Tensile |
MPa |
3021 |
GB/T 2568 |
Elongation at Break |
% |
3.92 |
GB/T 2568 |
Te Kaha Toka |
MPa |
115 |
GB/T 2570 |
Kōwae Takahuri |
MPa |
3540 |
GB/T 2570 |
Te Kaha Paanga |
KJ/M2 |
12.9 |
GB/T 2571 |
Barcol Hardness |
Barcol |
41 |
GB/T 3854 |
Tuhipoka:
1)Ko te tikanga tauira punaha whakarewanga ka mahia kia rite ki te GB/T 8237.
2)Pūnaha Whakaora: Hardener AKZO M-50: 1.5%; 0.6% Co-Naph 2%.
3) Whakaora i muri: RT × 24 h + 60 ℃ × 3h + 100 ℃ × 2h.
| Tono:
Ko te DP-1102D he pai mo te hanga i te paparanga o nga paipa FRP muka-whiu (sandwiched), tae atu ki te whakatakoto-a-ringa me nga hua FRP pultrusion.