DP-1060H Resin Puri-Rama mo te Maama Raarangi Fiberglass

Ko te kapia DP-1060H he mea hanga motuhake mo te hanga i nga awhi kaata kaata whakaahuru mura, ka tutuki nga whakaritenga mo te mura o te karaehe 1. He pai te tuku marama, te kaha o te miihini, me te mura o te mura, me nga taonga maaku-waho muka.
Wāteatanga:
  • DP-1060H

  • HUAKE

Whakaahuatanga Hua

Nga Taonga Matua me te Tono :

Taupānga: Ko te kapia DP-1060H he mea hanga motuhake mo te hanga i nga awhi kaata kaata whiti mo te mura, ka tutuki nga whakaritenga mo te mura o te karaehe 1. He pai te tuku marama, te kaha o te miihini, me te mura o te mura, me nga taonga maaku-waho muka.

Tikanga: E tika ana mo te hanga miihini me te whakatakoto-a-ringa i nga panui rama (tapa).

Tautukunga: E tutuki ana tenei hua ki te whakahau a te EU ROHS mo te mata, mercury, cadmium, hexavalent chromium, polybrominated biphenyl, me nga paerewa ihirangi polybrominated diphenyl ethers.


Nga Whakatakotoranga Hangarau o L iquid R esin:

Tūemi

Waeine

Tohutohu

Tikanga Whakamatau

Te ahua

---

Te wai marama kowhai marama

GB/T 8237.6.1.1

Poneke

25°C, cp

180-260

GB/T 7193.4.1

25°C GT

25°C, min

10-30

GB/T 7193.4.6

SPI-GT

min

1.0-2.0

HK-D-DB001

SPI-CT

min

2.6-4.0

HK-D-DB001

SPI-PET

°C

190-220

HK-D-DB001

Uara Waikawa

mgKOH/g

15.0-25.0

GB/T 2895

Tau Tae

Harzen

≤ 60

GB/T 605

Pūnaha whakaora i roto i te whakamātautau SPI: Accelerator KC: 2% Hardener M-50: 1.2%;


Maka Ahuatanga Tinana (hei tohutoro anake):

Tūemi

Waeine

Uara ine

Tikanga Whakamatau

Te Kaha Toka

MPa

50

GB/T 2568

Te Kaha Toka

MPa

90

GB/T 2570

Elongation at Break

%

3.7

GB/T 2568

Wera Distortion Temp

°C

60

GB/T 1634

Taurangi Hauora

%

30

GB/T 3854

Tuhipoka:

1) Ka hangaia te makanga kia rite ki te GB / T8237;

2) Whakatere (0.6% Co-Naph): 2%; Kai whakaora (AKZO M-50): 2%;

3) Ko nga tikanga i muri i te whakaora: RT × 24hrs + 60 ℃ × 3hrs + 100 ℃ × 2hrs.


Taupānga

| Tono:

Ko te DP-1060H he pai mo te hanga miihini me te hanga-a-ringa i nga panui rama (tapa).


D58134693(1)(1)

 Paewhiri Rama

D1288157_Whakaahua

Paewhiri Rama

Paewhiri Rama (3)_副本

Paewhiri Rama



DP-1060H TDS
Tōmua: 
Panuku: 

Nga korero e pa ana

he putua nga ihirangi!

Ohauru ki ta maatau Panui

Waiho to wahitau imeera ki te tiki i nga korero hua hou mai i ta maatau kamupene i nga wa katoa.
Ko Changzhou Huake polymer Co., Ltd. he tohungatanga ki te R&D, te whakaputa me te hoko o nga momo hua penei i te kapia polyester haunga, te kapia vinyl me etahi atu.

NGA LINKO Tere

NGA HUA

WHAKAARO

  +86- 19802502739
  marketing@huakepolymers.com
  No.602, Te Tai Tokerau Yulong Road,
Takiwa Xinbei, Changzhou City,
Jiangsu Province, Haina.
Mana pupuri © 2024 Changzhou Huake polymer Co., Ltd. Katoa nga mana pupuri. Tautokona e leadong.com     Mahere pae