+   86- 19802502739
marketing@huakepolymers.com<ci,=ut artifices summus qualitas eventus in variis partibus industriae regionibus consequi possit. ~!phoenix_var3_1!~
Products
Home » Mercatus » Aedificium & Construction » DP-1102D Polyester resinae unsaturated pro FRP Sheet et Pipes

loading

Share to:
facebook sharing button
Twitter sharing button
linea participatio puga
wechat sharing button
sharingin button sharing
pinterest sharing button
whatsapp sharing button
kakao sharing button
snapchat button sharing
sharethis sharing button

DP-1102D Unsaturated Polyester Resinae pro FRP Sheet et Pipes

Series DP-1102D est viscositas media, ortho-phthalica species polyester resinae nonsaturatae cum bona vi mechanica. Idoneum est ad fabricandum stratum fibrarum vulneris (sandwiched) fistulae FRP, necnon manus laicorum et pultrusionis formatorum FRP productorum. Inter eos, DP-1102D-Y ceram continet, nec DP-1102D-N ceram continet.
Availability:
  • DP-1102D

  • HUAKE

Product Description

Principalis Properties

Series DP-1102D est viscositas media, ortho-phthalica species polyester resinae nonsaturatae cum bona vi mechanica. Idoneum est ad fabricandum stratum fibrarum vulneris (sandwiched) fistulae FRP, necnon manus laicorum et pultrusionis formatorum FRP productorum. Inter eos, DP-1102D-Y ceram continet, nec DP-1102D-N ceram continet.


Specificationes Liquidae Resinae

Item

Unitas

Testimonium

Test Methodi

Aspectus

--

Lumine flavo liquidum pellucidum

GB/T 8237.6.1.1

Viscositas

25℃, cP

300-450

GB/T 7193.4.1

Gel Tempus

min

10.0-20.0

GB/T 7193.4.6

Firmus Content

%

60.0-68.0

GB/T 7193.4.3

*Curandi ratio in GT test: agentis curandi: AKZO M-50 2%; Promotor: 0.6% Co-Naph, 2%.


Physical P roperties of C asting (for reference only)

Item

Unitas

Metiri Value

Test Methodi

Calor Distortio Temperature

68

GB/T 1634

Distrahens fortitudo

MPa

70

GB/T 2568

Modulus distrahens

MPa

3021

GB/T 2568

Elongation at Break

%

3.92

GB/T 2568

Flexurae Fortitudo

MPa

115

GB/T 2570

Flexurale Modulus

MPa

3540

GB/T 2570

Fortitudo impulsum

KJ/M2

12.9

GB/T 2571

Barcol duritia

Barcol

41

GB/T 3854

Nota

1) Systema specimen methodi fundendi secundum GB/T 8237 exsecuta est.

2) Ratio curationis: Hardener AKZO M-50: 1.5%; 0.6% Co-Naph 2%.

3) Post curationem: RT × 24 h + 60℃×3h+100℃×2h.


Applicationem

|Applicationem:

DP-1102D apta est ad fabricandum stratum fibrarum vulneris (sandwiche) fistulae FRP, necnon manus laici et pultrusionis productorum formatorum FRP.


不透明板材

 Deponens Panel

_副本

Deponens Panel

_副本

Deponens Panel



DP-1102D TDS
Priora: 
Next: 

Related News

contentus inanis est!

Subscribe To Our Newsletter

Tuam electronicam electronicam relinque ut notitias uberrimas e societate nostra aliquo tempore recipias.
Changzhou Huake polymer Co, Ltd speciale in R & D, productio et venditio seriei productorum ut polyester resina unsaturated, resina vinyl et sic porro.

ORIGINAL LINKS

PRODUCTS

PRAECIPIO CONTRACTO

+   19802502739
marketing@huakepolymers.com marketing@huakepolymers.com
No.602  , North Yulong via,
Xinbei dolor, Changzhou urbem,
Jiangsu provinciae, Sinis.
Copyright © 2024 Changzhou Huake polymer Co, Ltd. All Rights Reserved. Supported by leadong.com     Sitemap