+86-18648932615
 marketing@huakepolymers.com
Products
Home » Markets » Musical Instrument » 20X-24N(formerly HS-8020N)Unsaturated Polyester Resin

loading

Share to:
facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
kakao sharing button
snapchat sharing button
sharethis sharing button

20X-24N(formerly HS-8020N)Unsaturated Polyester Resin

20X-24N resin (X indicates that the grade can be customized according to the customer's actual ambient temperature) is a spray resin specially used for wood coatings. Coated with wax-free thixotropic unsaturated polyester resin, it has excellent yellowing resistance, mirror luster, and can form an anti-sag coating. It is specially used in white pianos, musical instruments, speakers and other products, and the effect is excellent.
Availability:
  • 20X-24N(formerly HS-8020N)

  • HUAKE

Product Description

20X-24N(formerly HS-8020N)Unsaturated Polyester Resin

nPrincipal Properties & Application:

20X-24N resin (X indicates that the grade can be customized according to the customer's actual ambient temperature) is a spray resin specially used for wood coatings. Coated with wax-free thixotropic unsaturated polyester resin, it has excellent yellowing resistance, mirror luster, and can form an anti-sag coating. It is specially used in white pianos, musical instruments, speakers and other products, and the effect is excellent.


nSpecifications of liquid resin:

Item

Standard Requirements

Test Method

Appearance

Milky white translucent liquid

GB/T 8237.6.1.1

Viscosity(25℃, mPa.s)

350-500

GB/T 7193.4.1

Gel Time(min)

12-25

GB/T 7193.4.6

Thixotropic Index

2.4-3.5

GB/T 7193.4.1

Acid value (mgKOH/g)

10-25

GB/T 2895-2008

Solid Content (%)

52-56

GB/T 7193-2008

Water Content(%)

≤0.1

HK-D-DB007

Color Number(Hazen)

≤100

HK-D-DB036

The conditions for the testing of gel time: resin 50g; obalt 0.6% isooctanoate: 1.0 g; curing agent: AKZO M-50: 1.0 g.


Application
Application
TDS
Previous: 
Next: 

Related News

content is empty!

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap