Resin for Wood Coating HS-108SA

HS-108SA is a thixotropic unsaturated polyester resin specially used in wood coating by spraying. When used as varnish, it does not influence the transparence and has specular gloss and can also form a coating to prevent the sagging. It works best when used in the products such as pianos, musical instruments and speakers. The products produced by the resin has a high surface hardness and can form a thick and smooth coating. What’s more, its sandability and operability is both very good.
Availability:
  • HS-108SA

  • HUAKE

Product Description

Unsaturated polyester Resin HS-108(SA)

Principal Properties & Application:


HS-108SA is a thixotropic unsaturated polyester resin specially used in wood coating by spraying. When used as varnish, it does not influence the transparence and has specular gloss and can also form a coating to prevent the sagging. It works best when used in the products such as pianos, musical instruments and speakers. The products produced by the resin has a high surface hardness and can form a thick and smooth coating. What’s more, its sandability and operability is both very good.


Specifications of liquid resin:


Project

Unit

Index

Test Method

Appearance

---

Milky transparent liquid

GB/T 8237.6.1.1

Viscosity

25℃,mPa.s

400-500

HK-D-DB002

Gel Time

25℃, min

12.0-30.0

GB/T 7193.4.6

Thixotropic inde


2.4-3.5

HK-D-DB002

Curing system in GT test:Accelerator 0.6%Co/Naph: 2%;hardener AKZO M-50: 2%;



HS-108SA TDS
Application
Previous: 
Next: 

Related News

content is empty!

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap