HS-1026 Unsaturated Polyester Resin for FRP Lighting Panels

HS-1026 is a kind of unsaturated polyester resin specially used for making transparent FRP lighting panels, with good infiltration of glass fiber, good comprehensive mechanical strength and light transmittance, good aging resistance, and suitable for mechanism/hand lay-up process.
Availability:
  • HS-1026P

  • Huake

Product Description

HS-1026 Unsaturated Polyester Resin

Principal Properties & Application:

HS-1026 is a kind of unsaturated polyester resin specially used for making transparent FRP lighting panels, with good infiltration of glass fiber, good comprehensive mechanical strength and light transmittance, good aging resistance, and suitable for mechanism/hand lay-up process.

 

Specifications of liquid resin:

Item

    Unit

Standard Requirements

Test Method

Note

Appearance

――

Paste Liquid

GB/T8237.6.1.1


Viscosity(25℃, mPa.s)

25℃, CP

150-200

GB/T7193.4.1

11-3 月份

180-230

GB/T7193.4.1

4-5,9-10 月份

200-260

GB/T7193.4.1

6-8 月份

Gel Time

25℃, min

9.0-13.0

GB/T7193.4.6


Color Code

――

≦60

GB/T605

Harzen

 Curing system in SPI test: Hardener AKZO CH-50: 2%;

 

Physical properties of Casting(for reference only):

Item

Unit

Test Value

Test Method

Tensile Strength

MPa

70

GB/T 2568

Tensile Modulus of Elasticity

MPa

3200

GB/T 2568

Elongation at Break

%

2.8

GB/T 2568

Bending Strength

MPa

125

GB/T 2570

Bending Modulus of Elasticity

MPa

3650

GB/T 2570

Impact Strength

KJ/M2

10

GB/T 2571

Heat Distortion Temperature

℃

71

GB/T 1634

Barcol Hardness


47

GB/T 3854

1) Curing system: 0.6% Co-Naph 1%; MEKP 1%.

       2) Curing conditions after casting body: Normal temperature × 24h + 60℃ × 3h + 100℃ × 2h.

 

Precautions:

1) The product should be transported in accordance with the provisions on the transportation and unloading of chemical dangerous goods in Chapter 5 of the “Regulations on the Safety Administration of Chemical Dangerous Goods” of the State Council.

2) The product should be stored in a cool place under 25℃, avoid fire, isolate the heat source, and keep it sealed to prevent moisture intrusion and volatilization of monomer. the shelf life of the product is 3 months when stored under 25℃.

 


Previous: 
Next: 

Related News

content is empty!

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap