HS-1102E Unsaturated Polyester Resin for FRP Products

The HS-1102E series is an unsaturated polyester resin with medium reactivity, pre-accelerated, thixotropic, and good fiberglass wetting properties. It has excellent processing performance, smooth curing speed, and low shrinkage. The resin exhibits outstanding water resistance and good overall mechanical properties, making it suitable for hand lay-up/spray-up processes in the production of FRP products such as cockpit covers, automotive parts, and cooling towers.

 

This product complies with the EU RoHS directive concerning the content standards for lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls, and polybrominated diphenyl ethers.

Availability:
  • HS-1102E

  • Huake

Product Description

HS-1102E Unsaturated Polyester Resin

n Principal Properties & Application:

The HS-1102E series is an unsaturated polyester resin with medium reactivity, pre-accelerated, thixotropic, and good fiberglass wetting properties. It has excellent processing performance, smooth curing speed, and low shrinkage. The resin exhibits outstanding water resistance and good overall mechanical properties, making it suitable for hand lay-up/spray-up processes in the production of FRP products such as cockpit covers, automotive parts, and cooling towers.

 

This product complies with the EU RoHS directive concerning the content standards for lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls, and polybrominated diphenyl ethers.

 

n Specifications of liquid resin:

Item

Unit

Standard Requirements

Test Method

Appearance

--

Opaque liquid

GB/T 8237.6.1.1

Viscosity

25℃, cP

200-900

GB/T 7193.4.1

Gel Time

25℃, min

10-80

GB/T 7193.4.6

Solid Content

%

60-68

GB/T 7193.4.3

 Note: The curing system during the gel time test is: Curing agent AKZO M-50: 1%.

 

n Physical properties of Casting(for reference only):

Item

Unit

Test Value

Test Method

Tensile strength

MPa

58

GB/T 2568

Tensile Modulus

MPa

2800

GB/T 2568

Elongation at Break

%

2.0

GB/T 2568 

Flexural Strength

MPa

100

GB/T 2570

Flexural Modulus

MPa

3368

TB/T 2570

Impact Toughness

KJ/m²

6.3

GB/T 2571

HDT

℃

62

GB/T 1634

Barcol Hardness

--

40

GB/T 3854

 

Note:

1). The casting body preparation method follows GB/T 8237-2005. Curing system: AKZO M-50: 1.5%.

2). Post-curing system for the casting body: Room temperature (24 h) + 60°C (3 h) + 100°C (2 h).

 

 

 

n Precautions:

·  Users should select the appropriate type of resin based on specific environmental conditions and process requirements.

·  The HS-1102E series is a thixotropic resin. During storage, the thixotropic agent may settle, so it is recommended to gently stir before use to re-disperse it evenly.

·  The product should be stored in a cool place below 25°C, away from sources of ignition and heat (such as direct sunlight or steam), and the container should be sealed to prevent moisture and monomer evaporation. The shelf life at temperatures below 25°C is 3 months.


Previous: 
Next: 

Related News

content is empty!

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap