Low Shrink Additive HS-9817 for SMC/BMC

HS-9817 is a solution which made by dissolving the saturated polyester in styrene and has a medium viscosity.

Availability:
  • HS-9817

  • HUAKE

Product Description

Low Shrink Additive HS-9817 for SMC/BMC


Principal Properties & Application:

HS-9817 is a solution which made by dissolving the saturated polyester in styrene and has a medium viscosity.



Application:

HS-9817 is intended for low shrink SMC and BMC formulations with good surface quality. Depending on the choice and the ratio of UP-resin and high polymer, low shrinkage up to zero shrinkage can be achieved. The formulation can readily thickened with magnesium oxide. Its pigmenting property is limited. Recommended for the productions of electrics applications, automotive parts and etc.


Specifications of Liquid Resin:


Properties Range Test Method
Appearance Clear, light yellow HK-F-TM-00
Colour (Harzen) ≤60 HK-F-TM-01
Viscosity (25℃,Cp) 800-1000 HK-F-TM-03
Solid content (%) 66.0-68.0 HK-F-TM-08
Acid value (mgKOH/g) 4.0-5.5 HK-F-TM-09
Water content(%) <0.100 HK-F-TM-12


Technical Data Sheet
Application
Previous: 
Next: 

Related News

content is empty!

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap