HS-1500 Unsaturated Polyester Resin for SMC/BMC

HS-1500 is an unsaturated polyester resin used for SMC/BMC applications. It is made from maleic anhydride and standard diols as the main raw materials. This resin offers high reactivity, medium viscosity, and excellent thickening stability. When combined with low shrinkage agents such as HS-9892, HS-9812, and HS-9819, it produces high surface quality SMC/BMC products.

Availability:
  • HS-1500

  • Huake

Product Description

HS-1500 Unsaturated Polyester Resin

n Principal Properties & Application:

HS-1500 is an unsaturated polyester resin used for SMC/BMC applications. It is made from maleic anhydride and standard diols as the main raw materials. This resin offers high reactivity, medium viscosity, and excellent thickening stability. When combined with low shrinkage agents such as HS-9892, HS-9812, and HS-9819, it produces high surface quality SMC/BMC products.


n Specifications of liquid resin:

Item

Unit

Standard Requirements

Test Method

Appearance

---

Pale yellow transparent liquid

GB/T 8237.6.1.1

Viscosity

25℃, mPa.s

1450-1750

GB/T 7193.4.1

SPI-GT

min

4.0-8.0

HK-D-DB001

SPI-CT

min

5.5-10.5

HK-D-DB001

SPI-PET

℃

220-260

HK-D-DB001

Acid Value

mgKOH/g

13-19

GB/T 2895

Solid Content

%

63-68

GB/T 7193.4.3

  Moisture

%

≤0.15

HK-D-DB007

Color Index

---

≤80

HK-D-DB036

 Note: SPI: BPO paste 2%.

 

n Physical properties of Casting(for reference only):

Item

Unit

Measured Value

Test Method

Tensile Strength

MPa

50

GB/T 2568

Tensile Modulus

MPa

2900

GB/T 2568

Elongation at Break

%

1.2

GB/T 2568

Flexural Strength

MPa

90

GB/T 2570

Flexural Modulus

MPa

3300

GB/T 2570

Barcol Hardness

---

49

GB/T 3854

HDT

℃

130

GB/T 1634


Note:

1) Casting sample preparation follows GB/T 8237 with curing system: 0.6% Co-Naph 1.5%, AKZO M-50 1.5%..;

2) Curing process after casting: 24 hours at room temperature + 3 hours at 60°C + 2 hours at 110°C.

 

n Attention:

Ø During transportation, the product must comply with the provisions of the Regulations on the Safety Management of Hazardous Chemicals (Chapter 5, Regulations on the Transport and Handling of Hazardous Chemicals) issued by the State Council. The product should be stored in a cool, shaded place below 25°C, away from sources of ignition, and isolated from heat sources. It should be kept sealed to prevent moisture intrusion and the volatilization of monomers. The product has a shelf life of 3 months when stored at temperatures below 25°C.


Previous: 
Next: 

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap