Low Shrinkage Additive for SMC/BMC HS-9819C

HS-9819C is PVAC type low shrinkage additive for SMC/BMC, with magnesium oxide it can stabilise thickening and low shrinkage. It can be used with HS-1180, HS-1520, HS-1503 and other unsaturated polyester resins to get high surface quality products, but the colouring performance is limited.

Availability:
  • HS-9819C

  • Huake

Product Description

            Low Shrinkage Additive for SMC/BMC HS-9819C

n Characteristics and main uses:

HS-9819C is PVAC type low shrinkage additive for SMC/BMC, with magnesium oxide it can stabilise thickening and low shrinkage. It can be used with HS-1180, HS-1520, HS-1503 and other unsaturated polyester resins to get high surface quality products, but the colouring performance is limited.


n Technical indicators:

Item

Unit

Standard Requirements

Test Method

Appearance

--

Transparent - slightly turbid liquid

GB/T 8237.6.1.1

Viscosity

25℃ , mPa.s

5500-7500

HK-F-TM-05

Solid content

%

40.5-43.5

GB/T 7193.4.3

 

n Attention:

Ø Transportation should be in accordance with the provisions of the State Council's Regulations on the Safe Management of Dangerous Chemicals, Chapter 5, Transportation and Handling of Dangerous Chemical Substances. The product should be stored in a cool place under 25℃, avoid fire, isolate heat source, and keep it sealed to prevent moisture intrusion and volatilisation of monomer. Shelf life is 6 months when stored under 25℃. 


Previous: 
Next: 

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap