+86-18648932615
 marketing@huakepolymers.com
Products
Home » Markets » Moulding Resin » HS-4405 Epoxy Vinyl Ester Resin for Making General Fiberglass Molds

loading

Share to:
facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
kakao sharing button
snapchat sharing button
sharethis sharing button

HS-4405 Epoxy Vinyl Ester Resin for Making General Fiberglass Molds

HS-4405 is an epoxy vinyl ester resin that contains thixotropic agents and accelerators. It has low shrinkage, excellent dimensional stability, and smooth surface. The resin has good glass fiber wetting properties, is easy to apply, highly tough, crack-resistant, and has a high heat deflection temperature. It offers excellent thermal degradation resistance and superior strength retention at high temperatures. It is suitable for making general fiberglass molds.

Availability:
  • HS-4405

  • Huake

Product Description

HS-4405 Mold Resin

n Principal Properties & Application:

HS-4405 is an epoxy vinyl ester resin that contains thixotropic agents and accelerators. It has low shrinkage, excellent dimensional stability, and smooth surface. The resin has good glass fiber wetting properties, is easy to apply, highly tough, crack-resistant, and has a high heat deflection temperature. It offers excellent thermal degradation resistance and superior strength retention at high temperatures. It is suitable for making general fiberglass molds.

 

n Specifications of liquid resin:

Item

Unit

Standard Requirements

Test Method

Appearance

--

 

Red-purple, opaque liquid

GB/T 8237.6.1.1

Viscosity(25℃)

cp

250-350

GB/T 7193.4.1

Gel Time(25℃)

Min

15.0-55.0

GB/T 7193.4.6

 For gel time testing: Curing agent used is AKZO M-50, dosage 2%.

 

 n Physical properties of Casting(for reference only):

Item

Unit

Test Value

Test Method

Tensile Strength

MPa

80

GB/T 2567.5.1

Tensile Modulus

MPa

2900

GB/T 2567.5.1

Elongation at Break

%

4.5

GB/T 2567.5.1

Flexural Strength

MPa

125

GB/T 2567.5.3

Flexural Modulus

MPa

3000

GB/T 2567.5.3

Impact Toughness

KJ/m2

15.5

GB/T 2567.5.4

Barcol Hardness

---

38

GB/T 3854

HDT

℃

105

GB/T1634

 

Note:

1) The casting sample preparation method is according to GB/T 8237. Curing system: Curing agent M-50, 1.5%.

2) Curing treatment after casting: Room temperature for 24 hours + 60°C for 3 hours + 120°C for 2 hours.


n Precautions:

Ø Users should choose the appropriate type of resin based on specific environmental conditions and construction process requirements.

Ø  During transportation, the product should comply with Chapter 5 of the State Council's "Regulations on the Safety Management of Hazardous Chemicals" regarding the safe transportation of chemical hazardous materials.

Ø The product should be stored in a cool place below 25°C, away from sources of ignition and isolated from heat sources. The shelf life is 3 months when stored below 25°C.

 


Previous: 
Next: 

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap