HS-515 Solid Unsaturated Polyester Resin for dry SMC/BMC molding plastic products

HS-515 is a high-reactivity, crystalline solid unsaturated polyester resin that does not contain reactive monomers. It has strong crystallinity and is suitable for dry SMC/BMC molding plastic products. The products made from it have a long shelf life at room temperature, excellent electrical properties, and good water and chemical resistance.

Availability:
  • HS-515

  • Huake

Product Description

HS-515 Solid Unsaturated Polyester Resin

n Principal Properties & Application:

HS-515 is a high-reactivity, crystalline solid unsaturated polyester resin that does not contain reactive monomers. It has strong crystallinity and is suitable for dry SMC/BMC molding plastic products. The products made from it have a long shelf life at room temperature, excellent electrical properties, and good water and chemical resistance.

 

 

 

n Specifications of resin:

Item

Unit

Standard Requirements

Test Method

Appearance

--

White powder particles

GB/T 8237.6.1.1

Viscosity (200°C)

dPa · s

9.0-15.0

GB/T 7193.4.1

Acid Value

mgKOH/g

15.0-25.0

GB/T 2895

Melting Point

℃

100.0-115.0

GB/T 617

 

 

n Precautions:

      The product should be stored in a cool place at temperatures below 35°C, away from sources of ignition and heat. It should be sealed to prevent moisture absorption. The shelf life at temperatures below 35°C is 24 months.

 

 

 

 

 

 

 


Previous: 
Next: 

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap