+86-18648932615
 marketing@huakepolymers.com
Products
Home » Markets » SMC / BMC Resin » HS-917 Solid Unsaturated Polyester Resin for Dry SMC/BMC moulding products

loading

Share to:
facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
kakao sharing button
snapchat sharing button
sharethis sharing button

HS-917 Solid Unsaturated Polyester Resin for Dry SMC/BMC moulding products

HS-917 is a highly reactive, m-phenylene/neopentyl glycol type solid unsaturated polyester resin without reactive monomers, non-crystalline, and is suitable for use as a binder component for weftless tapes and BMC pellets, and the cured products have good heat resistance and electrical properties. Mixed with other solid resins, it can be used in dry SMC/BMC moulding products.

Availability:
  • HS-917

  • Huake

Product Description

HS-917 Solid Unsaturated Polyester Resin

 Characteristics and main uses:

HS-917 is a highly reactive, m-phenylene/neopentyl glycol type solid unsaturated polyester resin without reactive monomers, non-crystalline, and is suitable for use as a binder component for weftless tapes and BMC pellets, and the cured products have good heat resistance and electrical properties. Mixed with other solid resins, it can be used in dry SMC/BMC moulding products.

 Technical indicators:

Item

Unit

Standard Requirements

Test Method

Appearance

--

light yellow solid

GB/T 8237.6.1.1

Viscosity (200℃) (ICI Cone&Plate)

dPa · s

20.0-30.0

GB/T 7193.4.1

Acid value

mgKOH/g

15.0-25.0

GB/T 2895

Softening point

℃

80.0-100.0

GB/T 2294

 Attention:

The product should be stored in a cool place under 25℃, avoid fire, isolate the heat source, and keep it sealed to prevent moisture. When the temperature is high, especially in summer, the solid will be easily caked. Before use, the product should be heated and dissolved or crushed and then dissolved for use, and the shelf life is 12 months when stored under 25℃.


Previous: 
Next: 

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap