Isophthalic Type Unsaturated Polyester Resin HS-2223 for Bulk Molding Compound(BMC)

HS-2223 is an isophthalic type unsaturated polyester resin for Bulk Molding Compound(BMC), with high impact strength and toughness, as well as good electrical properties. It is applied in electrical components, industrial equipment and other fields.
Availability:
  • HS-2223

  • HUAKE

Product Description

Unsaturated Polyester Resin HS-2223

Principal Properties & Application: 

HS-2223 is an isophthalic type unsaturated polyester resin for Bulk Molding Compound(BMC), with high impact strength and toughness, as well as good electrical properties. It is applied in electrical components, industrial equipment and other fields.


Specifications of liquid resin:

Item

Standard Requirements

Test Method

Appearance

Light yellow transparent liquid

GB/T 8237.6.1.1

Viscosity(25℃, mPa.s)

2800-3200

GB/T 7193.4.1

SPI-GT(min)

5.5-7.5

HK-D-DB001

SPI-CT (min)

6.5-9.5

HK-D-DB001

SPI-PET(℃)

210-230

HK-D-DB001

Acid value (mgKOH/g)

11.0-14.0

GB/T 2895

Solid Content (%)

69-71

GB/T 7193.4.3

Water Content(%)

≤0.1

HK-D-DB007

Color Number(Hazen)

≤100

HK-D-DB036

Curing system in SPI test: Hardener AKZO CH-50: 2%

E-catalog
Application
Previous: 
Next: 

Related News

content is empty!

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap