Ko te HS-9819C he momo PVAC taapiri whakaheke iti mo te SMC / BMC, me te konupora konupora ka taea te whakapumau i te matotoru me te iti o te whakaheke. Ka taea te whakamahi me te HS-1180, HS-1520, HS-1503 me etahi atu kapia polyester haunga kore ki te tiki i nga hua kounga teitei o te mata, engari he iti te mahi tae.
| Wāteatanga: | |
|---|---|
HS-9819C
Huake
Whakapiri iti mo te SMC/BMC HS-9819C
n Nga ahuatanga me nga whakamahinga matua :
Ko te HS-9819C he momo PVAC taapiri whakaheke iti mo te SMC / BMC, me te konupora konupora ka taea te whakapumau i te matotoru me te iti o te whakaheke. Ka taea te whakamahi me te HS-1180, HS-1520, HS-1503 me etahi atu kapia polyester haunga kore ki te tiki i nga hua kounga teitei o te mata, engari he iti te mahi tae.
n Tohu Hangarau :
Tūemi |
Waeine |
Nga Whakaritenga Paerewa |
Tikanga Whakamatau |
Te ahua |
-- |
Puataata - he wai kerekere |
GB/T 8237.6.1.1 |
Poneke |
25 ℃ , mPa.s |
5500-7500 |
HK-F-TM-05 |
Te ihirangi totoka |
% |
40.5-43.5 |
GB /T 7193.4.3 |
n Te aro :
Ø Ko te kawe waka kia rite ki nga tikanga o nga Ture a te Kaunihera a te Kawanatanga mo te Whakahaere Haumaru o nga Matū Kino, Upoko 5, Te Kawenata me te Whakahaerenga o nga Matū Whakamate. Me penapena te hua ki te waahi hauhautanga i raro i te 25 ℃ , karohia te ahi, wehe i te puna wera, kia hiritia kia kore ai e uru mai te makuku me te wawaotanga o te monomer. He 6 marama te roa o te wa ka penapena i raro i te 25 ℃.