Ko te HS-1500 he kapia polyester haunga e whakamahia ana mo nga tono SMC/BMC. He mea hanga mai i te maleic anhydride me nga diol paerewa hei rauemi mata matua. Ko tenei kapia he nui te tauhohenga, te pokey reo, me te tino pumau o te matotoru. I te wa e hono ana ki nga kaihoko whakaheke iti penei i te HS-9892, HS-9812, me te HS-9819, ka puta mai nga hua SMC / BMC teitei o te mata.
| Wāteatanga: | |
|---|---|
HS-1500
Huake
HS-1500 Resin Polyester Kore Hanga
n Nga Taonga Matua me te Tono :
Ko te HS-1500 he kapia polyester haunga e whakamahia ana mo nga tono SMC/BMC. He mea hanga mai i te maleic anhydride me nga diol paerewa hei rauemi mata matua. Ko tenei kapia he nui te tauhohenga, te pokey reo, me te tino pumau o te matotoru. I te wa e hono ana ki nga kaihoko whakaheke iti penei i te HS-9892, HS-9812, me te HS-9819, ka puta mai nga hua SMC / BMC teitei o te mata.
n Nga korero mo te kapia wai :
Tūemi |
Waeine |
Nga Whakaritenga Paerewa |
Tikanga Whakamatau |
Te ahua |
--- |
Te wai maramara kowhai kowhai |
GB /T 8237.6.1.1 |
Poneke |
25 ℃ , mPa.s |
1450-1750 |
GB /T 7193.4.1 |
SPI-GT |
min |
4.0-8.0 |
HK -D- DB001 |
SPI-CT |
min |
5.5-10.5 |
HK -D- DB001 |
SPI-PET |
℃ |
220-260 |
HK -D- DB001 |
Uara Waikawa |
mgKOH/g |
13-19 |
GB /T 2895 |
Ihirangi Mārō |
% |
63-68 |
GB /T 7193.4.3 |
makuku |
% |
≤0.15 |
HK -D- DB007 |
Taurangi Tae |
--- |
≤80 |
HK -D- DB036 |
Tuhipoka: SPI : BPO whakapiri 2%.
n Ngā āhuatanga ā-tinana o te whakangao C (hei tohutoro anake) :
Tūemi |
Waeine |
Uara ine |
Tikanga Whakamatau |
Te Kaha Toka |
MPa |
50 |
GB/T 2568 |
Kōwae Tensile |
MPa |
2900 |
GB/T 2568 |
Elongation at Break |
% |
1.2 |
GB/T 2568 |
Te Kaha Toka |
MPa |
90 |
GB/T 2570 |
Kōwae Takahuri |
MPa |
3300 |
GB/T 2570 |
Barcol Hardness |
--- |
49 |
GB/T 3854 |
HDT |
℃ |
130 |
GB/T 1634 |
Tuhipoka :
1) Ka whai te whakarite tauira makanga i te GB/T 8237 me te punaha whakaora: 0.6% Co-Naph 1.5%, AKZO M-50 1.5%.;
2) Te tukanga whakaora i muri i te maka: 24 haora i te pāmahana rūma + 3 haora i te 60 ° C + 2 haora i te 110 ° C.
n Te aro :
Ø I te wa o te waka, me whai te hua ki nga tikanga o nga Ture mo te Whakahaere Haumarutanga o nga Matū Morearea (Wapoko 5, Ture mo te Kawea me te Whakahaere o nga Matū Morearea) i tukuna e te Kaunihera o te Kawanatanga. Me penapena te hua ki roto i te waahi matao, marumaru i raro i te 25 ° C, mawehe atu i nga puna o te mura, me te wehe mai i nga puna wera. Me hiri tonu kia kore ai e uru mai te makuku me te wawaotanga o nga monomers. E 3 marama te roa o te hua ka penapena ki nga mahana i raro iho i te 25 ° C.