Unsaturated Polyester Resin Flame Retardancy RTM Process HS-307C-GY

1)HS-307C-GY is an unsaturated Polyester Resin with flame resistance.
2)Pre-accelerated,fluidity and excellent glass infiltration resistance.
3)Suitable for vaccum infusion molding ,RTM process.
Availability:
  • HS-307C-GY

  • HUAKE

Product Description

HS-307C-GY  Unsaturated Polyester Resin

  • Principal Properties

1)HS-307C-GY is an unsaturated Polyester Resin with flame resistance.

2)Pre-accelerated,fluidity and excellent glass infiltration resistance.

3)Suitable for vaccum infusion molding, RTM process.


  • Typical Liquid Resin Properties:

Properties

Unit

Value

Test Method

Appearance

--

Blue transparent or micro muddy liquids

GB/T 8237.6.1.1

Viscosity

25℃,cps

180-220

GB/T 7193.4.1

*Gel-time

25℃,min

70.0-80.0

GB/T 7193.4.6



Solid content


%

50.0-60.0

GB/T 7193.4.3

*Curing agent: AKZO M-50 1.5%.


Properties of Glass Fiber Laminated (Typical Values) :


Fire Resistance Properties



Value



Test Method



Limited Oxygen Index(%)



31.5



GB/T 2406



Note:

  1) Samples-making according to GB/T8237-2005,Curing agent AKZO M-50 1.5%.



  2)Casting Postcure:RT×24hrs+60℃×1hrs+80℃×4hrs.



  3)9 layers of 400g/m2 glass fiber cloth.



HS-307C TDS
Previous: 
Next: 

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap