Kore Haanga Polyester Resin Muri Retardancy RTM Tukanga HS-307C-GY

1) Ko te HS-307C-GY he Resin Polyester haunga me te aukati mura.
2)I mua i te tere, te wai me te pai o te karaehe whakaurunga atete.
3) He pai mo te hangai whaowhia marua, te tukanga RTM.
Wāteatanga:
  • HS-307C-GY

  • HUAKE

Whakaahuatanga Hua

HS-307C-GY Resin Polyester Hangakore

  • Nga Taonga Matua

1) Ko te HS-307C-GY he Resin Polyester haunga me te aukati mura.

2)I mua i te tere, te wai me te pai o te karaehe whakaurunga atete.

3) He pai mo te hangai whaowhia marua, te tukanga RTM.


  • Ngā Āhuatanga Resin Liquid:

Āhuatanga

Waeine

Uara

Tikanga Whakamatau

Te ahua

--

He kikorangi, he wai paru moroiti ranei

GB/T 8237.6.1.1

Poneke

25℃, cps

180-220

GB/T 7193.4.1

*Wa-wa

25℃, min

70.0-80.0

GB/T 7193.4.6



Te ihirangi totoka


%

50.0-60.0

GB/T 7193.4.3

*Kaiwhakaora: AKZO M-50 1.5%.


Ngā Āhuatanga o te Karāhe Fiber Laminated (Uara Tikanga) :


Āhuatanga ātete ahi



Uara



Tikanga Whakamatau



Taupū hāora iti(%)



31.5



GB/T 2406



Tuhipoka:

  1) Tauira-hanga rite ki GB / T8237-2005, Curing kaihoko AKZO M-50 1.5%.



  2)Te Makanga Whakamutunga:RT×24 haora+60℃×1haora+80℃×4haora.



  3)9 paparanga o 400g/m .2 te kakahu muka karaihe



HS-307C TDS
Tōmua: 
Panuku: 

Changzhou Huake Polymer Co., Ltd.

I whakapau kaha a Huake ki te whakarato ki nga kaihoko nga hua o te kounga teitei me nga otinga matawhānui i roto i te mara o nga rauemi hiato me nga taapiri na roto i nga mahi hangarau.
Ko Changzhou Huake polymer Co., Ltd. he tohungatanga ki te R&D, te whakaputa me te hoko o nga momo hua penei i te kapia polyester, te kapia vinyl me etahi atu.

NGA LINKO Tere

NGA HUA

WHAKAARO

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Mana pupuri © 2024 Changzhou Huake polymer Co., Ltd. Katoa nga mana pupuri. Tautokona e leadong.com     Mahere pae