Gelcoat HS-NC7035S/H

HS-NC7035S/H Gelcoat is an IPA/NPG type gel coat, which matrix resin is isophthalic acid/neopentyl glycol unsaturated polyester, and it is pre-promoted. The structure of the matrix resin endows the gel coat with good mechanical properties and weather resistance, so this gel coat is especially suitable for the fields with high requirements of weather resistance and water resistance. "7035"represents the color number.

Availability:
  • HS-NC7035S/H

  • HUAKE

Product Description

Gelcoat HS-NC7035S/H

Principal Properties & Application:

HS-NC7035S/H Gelcoat is an IPA/NPG type gel coat, which matrix resin is isophthalic acid / neopentyl glycol unsaturated polyester, and it is pre-promoted. The structure of the matrix resin endows the gel coat with   good mechanical properties and weather resistance, so this gel coat is especially suitable for the fields with high requirements of weather resistance and water resistance. “7035” represents the color number.

>     Excellent impact resistance;

>     Very high surface gloss;

>     Excellent water resistance and weather resistance;

>     Excellent high temperature resistance and corrosion resistance.

Applications:

Suitable for ships, buildings, vehicles, wind power, swimming pools, sanitary ware and other fields.


Specifications of Liquid Gelcoat:


Test Item

Unit

Test Value

Test Method

Appearance

——

Gray paste liquid

--

Viscosity (25℃)

CP

6000-9000 (S)

10000-13000 (H)

ISO 2555 Brookfield RV

/DV-I Spindle 6-10 RPM

Gel time(25℃)

min

5.0-15.0 (S)

10.0-20.0 (H)

ISO 2535

Solid content

%

58.0-66.0

NF751-515

Thixotropic index

——

≥3.5

ISO 2555 Brookfield RV/DV-I

Gel time test: Curing agent M-50(AKZO)2%;S: Spray type;H: Brush type.


Technical Data Sheet
Application
Previous: 
Next: 

Related News

content is empty!

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap