| Wāteatanga: | |
|---|---|
HS-9800-35S
HUAKE
Nga Taonga Matua me te Tono :
Ko te HS-9800-35S he whakamaarama wai motuhake mo te SMC / BMC, e whakaatu ana i te whakamararatanga pai me te pumau o te matotoru. Ko te whakakoi wai e pupuri ana i te pumau mo te wa roa i roto i nga mahi, me te whakarite kia pai ake nga hua o te SMC / BMC ki te pai ake o te rere me te kounga i muri i te whakamahinga.
Tohu Hangarau mo te Wai Thickener :
Tūemi |
Waeine |
Tohutohu |
Tikanga Whakamatau |
Te ahua |
--- |
Whakapiri, kaore he mea ke |
GB/T 8237.6.1.1 |
Poneke |
25℃, mPa.s |
14000-22000 |
HK-F-TM-06 |
Ihirangi konupora oxide |
% |
34-36 |
HK-D-DB026 |
Whakatupato:
Ko te HS-9800-35S he punaha marara o te whakakii konupora waikura me te kapia kawe. I te wa e rokiroki ana, ka tau pea te konupora waikura i etahi wa. Me tino whakakorikori i te whakakorikori i roto i te oko i mua i te whakamahi kia kore ai e pa ki te paanga whakapawera.
Me ū nga waka ki nga ture kawe waka me te utaina mo nga matū morearea pera i tuhia i roto i te Upoko 5 o te 'Regulations on the Safe Management of Hazardous Chemicals' a te Kaunihera.
Me penapena te hua ki te waahi hauhautanga i raro iho i te 25 ℃, matara atu i te ahi, mawehe mai i nga puna wera, ka hiri kia kore ai e uru mai te makuku me te wawaotanga o te monomer. E 6 marama te roa o te wa ka penapena ki raro i te 25 ℃.