HS-2250 Unsaturated Polyester Resin for The Production of Large-scale Products

HS-2250 is an unsaturated polyester resin specially designed for polyester concrete. It has low viscosity, low shrinkage, good wettability with fillers to maintain a high filler rate, low volatilisation of styrene to improve the working environment, excellent workability, good air-drying property, which prevents sticking on the surface of the moulded products in a short time and forms a glossy and smooth surface. It is suitable for the production of large-scale products.

Availability:
  • HS-2250

  • Huake

Product Description

HS-2250 Unsaturated Polyester Resin

n Characteristics and main uses:

HS-2250 is an unsaturated polyester resin specially designed for polyester concrete. It has low viscosity, low shrinkage, good wettability with fillers to maintain a high filler rate, low volatilisation of styrene to improve the working environment, excellent workability, good air-drying property, which prevents sticking on the surface of the moulded products in a short time and forms a glossy and smooth surface. It is suitable for the production of large-scale products.

n Specifications of liquid resin:

Item

Unit

Standard Requirements

Test Method

Appearance

--

yellow transparent liquid

GB/T 8237.6.1.1

Viscosity

25℃, cP

130-170

GB/T 7193.4.1

Gel Time

25℃, min.

5.0-13.0

GB/T 7193.4.6

 The curing system for testing the gel time was: accelerator 6% Co/Naph: 1%; curing agent AKZO M-50: 2%.

n Physical properties of Casting(for reference only):

Item

Unit

Test Value

Test Method

Tensile strength

MPa

41

GB/T2568

Tensile modulus

MPa

2949

GB/T2568

Elongation at break

%

1.53

GB/T2568

Bending strength

MPa

61

GB/T2570

Bending modulus

MPa

3121

GB/T2570

Impact toughness

KJ/m2

3.24

GB/T2571

Bacall hardness

--

40

GB/T3854

Heat distortion temperature

℃

62

GB/T1634

Note:

1) Pouring method is according to GB/T8237-2005. Curing system: accelerator HS-909 1.5%, AKZO M-50: 1.5%;

2) Curing system after casting body: Normal temperature (24 h) + 60°C (3 h) + 100°C (2 h).

n Refer to the recipe for use:

                                            parts by weight

HS-2250 resin                                                                                                                              100parts

Accelerator HS-995                                       2parts

Curing agent (methyl ethyl ketone peroxide MEKPO)               1-2 parts (dosage depends on temperature)

Calcium carbonate / silica sand and other fillers                        600parts

n Attention:

1. When the temperature of construction environment is high, the gel time is short, at this time, you can not arbitrarily reduce the amount of curing agent, but should reduce the amount of accelerator.

2. Because of the low shrinkage rate of the resin, in order to prevent the mould release difficulty, so it is recommended to use polyvinyl alcohol or fluorine type mould release agent.

Transportation should be in accordance with the State Council ‘Regulations on the Safe Management of Chemical Dangerous Goods’, Chapter V of the transport and handling of chemical dangerous goods. The product should be stored in a cool place under 25℃, avoid fire, isolate the heat source (such as direct sunlight or steam, etc.), and keep the barrel sealed to prevent moisture intrusion and volatilisation of the monomer.The shelf life is 3 months when stored under 25℃.


Previous: 
Next: 

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18014995084
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap