HS-2250 Resin Polyester Kore Hanga mo te Whakangaotanga o nga Hua Nui

Ko te HS-2250 he kapia polyester haunga i hangaia mo te raima polyester. He iti te viscosity, he iti te whakaheke, he pai te makuku me te whakakii ki te pupuri i te reeti whakakii teitei, te iti o te whakahekenga o te styrene ki te whakapai ake i te taiao mahi, te pai o te mahi, te pai o te whakamaroke hau, e kore ai e piri ki runga i te mata o nga hua i whakarewahia i roto i te wa poto ka hanga he mata kanapa me te maeneene. He pai mo te hanga i nga hua nui.

Wāteatanga:
  • HS-2250

  • Huake

Whakaahuatanga Hua

HS-2250 Resin Polyester Hangakore

n  Nga ahuatanga me nga whakamahinga matua :

Ko te HS-2250 he kapia polyester haunga i hangaia mo te raima polyester. He iti te viscosity, he iti te whakaheke, he pai te makuku me te whakakii ki te pupuri i te reeti whakakii teitei, te iti o te whakahekenga o te styrene ki te whakapai ake i te taiao mahi, te pai o te mahi, te pai o te whakamaroke hau, e kore ai e piri ki runga i te mata o nga hua i whakarewahia i roto i te wa poto ka hanga he mata kanapa me te maeneene. He pai mo te hanga i nga hua nui.

n  Nga korero mo te kapia wai :

Tūemi

Waeine

Nga Whakaritenga Paerewa

Tikanga Whakamatau

Te ahua

--

wai maramara kowhai

GB/T 8237.6.1.1

Poneke

25, cP

130-170

GB/T 7193.4.1

G el T ime

25, min.

5.0-13.0

GB/T 7193.4.6

 Ko te punaha whakaora mo te whakamatautau i te wa ra ko: whakatere 6% Co/Naph: 1%; kaihoko whakaora AKZO M-50: 2%.

n  Ngā āhuatanga ā-tinana o te whakangao C (hei tohutoro anake) :

Tūemi

Waeine

Uara Whakamatau

Tikanga Whakamatau

Te kaha tensile

MP a

41

GB/T2568

Kohikohiko tensile

MPa

2949

GB/T2568

Te whakaroa i te wehenga

%

1.53

GB/T2568

Te kaha piko

MPa

61

GB/T2570

Kōwae piko

MPa

3121

GB/T2570

Te pakari o te paanga

KJ/m2

3.24

GB/T2571

te pakeke o Bacall

--

40

GB/T3854

Te wera o te wera

62

GB/T1634

Tuhipoka:

1) Ko te tikanga ringihia ki te GB / T8237-2005. Pūnaha whakaora: whakatere HS-909 1.5%, AKZO M-50: 1.5%;

2) Pūnaha whakaora i muri i te makanga tinana: Te pāmahana noa (24 h) + 60 ° C (3 h) + 100 ° C (2 h).

n  Tirohia te tohutao mo te whakamahi:

                                            nga waahanga ma te taumaha

HS-2250  kapia 100waahanga

Whakatere HS-995                                        2waahanga

Kai whakaora (methyl ethyl ketone peroxide MEKPO)                1-2 nga wahanga (kei runga i te pāmahana te horopeta)

Te konupora warowaiha / kirikiri kirikiri me etahi atu whakakii                         600 nga waahanga

n  Te aro :

1. A, no te tiketike o te pāmahana o te taiao hanga, he poto te wa gel, i tenei wa, e kore e taea e koe te whakaiti i te nui o te kaihoko whakaora, engari me whakaiti i te nui o te whakatere.

2. B na te iti o te whakahekenga o te kapia, hei aukati i te uaua o te tuku i te pokepokea ai, na reira ka tūtohutia kia whakamahia te waipiro polyvinyl, te momo fluorine mo te tuku i te maaka.

Ko nga waka e tika ana kia rite ki nga Ture a te Kaunihera a te Kawanatanga mo te Whakahaere Haumaru o nga Taonga Whakamate Matū , Upoko V o te kawe me te whakahaere i nga taonga kino matū. Me penapena te hua ki te waahi hauhautanga i raro i te 25 , karohia te ahi, wehe i te puna wera (penei i te ra tika, te mamaoa ranei, me etahi atu), me te pupuri i te oko hiri kia kore ai e uru mai te makuku me te pahekeheke o te monomer ..


Tōmua: 
Panuku: 

Ohauru ki ta maatau Panui

Waiho to wahitau imeera ki te tiki i nga korero hua hou mai i ta maatau kamupene i nga wa katoa.
Ko Changzhou Huake polymer Co., Ltd. he tohungatanga ki te R&D, te whakaputa me te hoko o nga momo hua penei i te kapia polyester haunga, te kapia vinyl me etahi atu.

NGA LINKO Tere

NGA HUA

WHAKAARO

  +86- 19802502739
  marketing@huakepolymers.com
  No.602, Te Tai Tokerau Yulong Road,
Takiwa Xinbei, Changzhou City,
Jiangsu Province, Haina.
Mana pupuri © 2024 Changzhou Huake polymer Co., Ltd. Katoa nga mana pupuri. Tautokona e leadong.com     Mahere pae