Home » Mercatus » Resinae speciales » HS-2250 Resinae Polyester unsaturated pro productione magnarum productarum

loading

Share to:
facebook sharing button
Twitter sharing button
linea participatio puga
wechat sharing button
sharingin button sharing
pinterest sharing button
whatsapp sharing button
kakao sharing button
snapchat button sharing
sharethis sharing button

HS-2250 unsaturated Polyester Resinae productione magnarum Products

HS-2250 est polyester resina unsaturata ad concreta polyester specialiter destinata. Habet viscositatem, humilem DECREMENTUM, bonam wettability cum fillers tenere altam ratem, humilem volatilisationem styrene ad emendare opus ambitus, excellentem operabilitatem, bona aeris siccantia proprietas, quae in superficie productorum formatorum brevi haerere prohibet et superficies nitida et leni formatur. Idoneum est ad productionem rerum magnarum.

Availability:
  • HS-2250

  • Huake

Product Description

HS-2250 unsaturated Polyester Resinae

n  Characteres et usus principalis

HS-2250 polyester resina unsaturated est concreta polyester specialiter destinata. Habet viscositatem, humilem DECREMENTUM, bonam wettability cum fillers tenere altam ratem, humilem volatilisationem styrene ad emendare opus ambitus, excellentem operabilitatem, bona aeris siccantia proprietas, quae in superficie productorum formatorum brevi haerere prohibet et superficies nitida et leni formatur. Idoneum est ad productionem rerum magnarum.

n :  Specificationes liquidae resinae

Item

Unitas

Latin Requisita

Test Methodi

Aspectus

--

flavo liquido

GB/T 8237.6.1.1

Viscositas

25cP,

130-170

GB/T 7193.4.1

G el T ime

25, min .

5.0-13.0

GB/T 7193.4.6

 Ratio sanandi tentandi tempus gel fuit: accelerator 6% Co/Naph: 1%; curandi agentis AKZO M- L:2%.

n  Physica de C asting for reference only)(

Item

Unitas

Test Precium

Test Methodi

distrahentes vires

MP a

41

GB/T2568

Modulus distrahens

MPa

2949

GB/T2568

Prolongatio ad intermissum

%

1.53

GB/T2568

vires tendentes

MPa

61

GB/T2570

inflexio modulus

MPa

3121

GB/T2570

Impulsum spissitudo

KJ/m2

3.24

GB/T2571

Persius duritia

--

40

GB/T3854

Calor tortor tortor

62

GB/T1634

Nota:

1) Methodus fundendi secundum GB/T8237-2005 est. Ratio sanandi: accelerator HS-909 1.5%, AKZO M-50: 1.5%;

2) Systema curandi post corpus dejectum: Temperatura normalis (24 h) + 60 ° C (3 h) + 100 ° C (2 h).

n  Quaere recipe pro usu;

                                            partes pondere

HS-2250  resinae 100parts

Accelerator HS-995                                        2parts

Agens curans (methyl keton peroxide MEKPO)                partes 1-2 (dosis a temperatus pendent)

Calcium carbonas / silica arena et aliae                         600partes fillers

n  Operam :

1. Cum temperatura constructionis ambitus altus est, tempus gel breve est, hoc tempore, non quantum ad arbitrium agentis sanationis minuere, sed acceleratoris quantitatem minuere.

2. B propter humilitatem DECREMENTUM rate resinae, ut difficultas emissio formae ne, ita commendatur ut polyvinyl alcohol vel fluorine speciei formae emissio agentis utatur.

Transportatio secundum Constitutiones Concilii publicae de bonis chemicis periculosis tutus procuratio , Caput V de bonis periculosis chemicis et de cariandis pertractandis. Productum in loco frigido sub 25 condi debet , ignem vitare, fontem caloris segregare (ut directum solis vel vaporis, etc.), et dolium signatum servare ne humorem intrusionem et volatilisationem monomer ..


Previous: 
Next: 

Subscribe To Our Newsletter

Tuam electronicam electronicam relinque ut notitias uberrimas e societate nostra aliquo tempore recipias.
Changzhou Huake polymer Co, Ltd speciale in R & D, productio et venditio seriei productorum ut polyester resina unsaturated, resina vinyl et cetera.

ORIGINAL LINKS

PRODUCTS

PRAECIPIO CONTRACTO

+   19802502739
marketing@huakepolymers.com marketing@huakepolymers.com
No.602  , North Yulong via,
Xinbei dolor, Changzhou urbem,
Jiangsu provinciae, Sinis.
Copyright © 2024 Changzhou Huake polymer Co, Ltd. All Rights Reserved. Supported by leadong.com     Sitemap