Adhesive for Solar Photovoltaic Backsheet HN-1725 Series

This product is the hydroxyl component of a solvent-based two-component polyurethane adhesive, which can be used in high-performance solar cell backplanes when combined with an isocyanate curing agent. It has excellent adhesion to well-treated PVDF film, PVF film, PE film, PET film, etc., short curing time, high initial strength, and excellent resistance to heat and moisture, passing PCT 96h and DH 3000h tests.

Availability:
  • HN-1725B

  • HUAKE

Product Description

Adhesive for Solar Photovoltaic Backsheet HN-1725 Series


Principal Properties & Application:

This product is the hydroxyl component of a solvent-based two-component polyurethane adhesive, which can be used in high-performance solar cell backplanes when combined with an isocyanate curing agent. It has excellent adhesion to well-treated PVDF film, PVF film, PE film, PET film, etc., short curing time, high initial strength, and excellent resistance to heat and moisture, passing PCT 96h and DH 3000h tests.



Product Characteristics:

Model

HN-1725

HN-1725B

Appearance

Clear transparent viscous liquid

Clear transparent viscous liquid

Color (Pt-Co)

≤ 80

≤ 80

Acid Value (mgKOH/g)

< 1

< 1

Hydroxyl Value (mgKOH/g)

11-15

8-12

Solid Content (%)

50%

50%

Viscosity (25℃, mPa.s)

50-200

50-200

Main Curing Ratio (based on N3300)

22/1

30/1



Recommended Application Process:

Coating Method: Suitable for mainstream coating methods such as mesh coating, scraper, and extrusion.

Oven Temperature: 80-120 °C

Solid Content for Machine: It is recommended to dilute with ethyl acetate to 30-45% solid content for machine use.

Coating Dry Weight: It is recommended 6-10 g/m², dry film thickness 6-10μm.

Curing Conditions: Cure at 50°C for 48 hours or at 35°C for 3-4 days. Adjust and customize according to customer processes.


Application
HN-1725B TDS
Previous: 
Next: 

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap