Tenaces pro Solario Photovoltaico Backsheet HN-1725 Series

Productum hoc est hydroxyli componentis duo-componentis polyurethani tenaces soluti fundati, quae adhiberi potest in summo faciendo cella solaris backplana cum coniunctione cum agente curatione isocyanate. Praeclara adhaesio ad movendum bene tractatum PVDF velum, PVF velum, PE velum, PET velum, etc., breve tempus sanationis, vires initiales altas, et calori et humori praecellens resistentiam, transiens PCT 96h et DH 3000h probat.

Availability:
  • HN-1725B

  • HUAKE

Product Description

Tenaces pro Solario Photovoltaico Backsheet  HN-1725 Series


Properties & ApplicationPrincipal

Productum hoc est hydroxyli componentis duo-componentis polyurethani tenaces soluti fundati, quae adhiberi potest in summo faciendo cella solaris backplana cum coniunctione cum agente curatione isocyanate. Praeclara adhaesio ad movendum bene tractatum PVDF velum, PVF velum, PE velum, PET velum, etc., breve tempus sanationis, vires initiales altas, et calori et humori praecellens resistentiam, transiens PCT 96h et DH 3000h probat.



Product Characteres

Exemplar

HN-1725

HN-1725B

Aspectus

Liquidum viscosum perspicuum perspicuum est

Liquidum viscosum perspicuum perspicuum est

Color (Pt-Co)

≤ 80

≤ 80

Acidum valorem (mgKOH/g)

< 1

< 1

Hydroxyl Value (mgKOH/g)

11-15

8-12

Firmus Contentus (%)

L%

L%

Viscositas (25℃, mPa.s)

50-200

50-200

Main Curing Ratio (secundum N3300)

22/1

30/1



Commendatur Application processum:

Modus efficiens: Apta pro amet efficiens modi ut reticulum efficiens, strigili, et extrusio.

Oven Temperature: 80-120 °C

Solidum Content pro Machina: Commendatur ad 30-45% solidi contenti ad usum machinae diluendum cum ethyl acetate.

Pondus siccum efficiens: Commendatur 6-10 g/m², crassities pelliculae aridae 6-10μm.

Condiciones sanans: Curator in 50°C pro 48 horis vel 35°C pro 3-4 diebus. Adjust and customize according to customer process.


Applicationem
HN-1725B TDS
Priora: 
Next: 

Changzhou Huake Polymer Co., Ltd.

Huake semper deditus est ut clientibus qualitatibus productis et solutionibus comprehensivis in campo materiae compositae et adhaesivis per innovationem technologicam comparandis.
Changzhou Huake polymer Co, Ltd speciale in R & D, productio et venditio seriei productorum ut polyester resina unsaturated, resina vinyl et cetera.

ORIGINAL LINKS

PRODUCTS

PRAECIPIO CONTRACTO

  +86-19802503183
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei dolor, Changzhou urbem,
Jiangsu provinciae, Sinis.
Copyright © 2024 Changzhou Huake polymer Co, Ltd. All Rights Reserved. Supported by leadong.com     Sitemap