Acrylic Resin for Solar Backsheet Coating HN-2604 Series

The HN-2604 Series is a solvent-based acrylic resin that, when combined with an isocyanate curing agent, can be used in high-performance solar photovoltaic backsheet coatings. It has excellent compatibility with various types of trifluorinated and tetrafluorinated FEVE resins, allowing for blending in any ratio to reduce fluorine content and save costs. It also offers excellent adhesion to PET and EVA substrates, and performs well in humidity and heat aging, passing the PCT 48h aging test with proper formulation. The resin exhibits excellent mechanical properties and can be directly used in the grinding of coatings.
Availability:
  • HN-2604 Series

  • Huake

Product Description

Acrylic Resin for Solar Backsheet Coating

HN-2604 Series

n Product Introduction:

The HN-2604 Series is a solvent-based acrylic resin that, when combined with an isocyanate curing agent, can be used in high-performance solar photovoltaic backsheet coatings. It has excellent compatibility with various types of trifluorinated and tetrafluorinated FEVE resins, allowing for blending in any ratio to reduce fluorine content and save costs. It also offers excellent adhesion to PET and EVA substrates, and performs well in humidity and heat aging, passing the PCT 48h aging test with proper formulation. The resin exhibits excellent mechanical properties and can be directly used in the grinding of coatings.

n Product Characteristics:

Item

HN-2604A

HN-2604L

Appearance

Colorless to pale yellow transparent viscous liquid

Colorless to pale yellow transparent viscous liquid

Color (Pt-Co)

≤40

≤40

Acid Value (mg KOH/g)

5-7

4-7

Hydroxyl Value (mg KOH/g)

23-33

25-35

Solid Content* (%)

58-62

58-62

Viscosity (25℃, mPa·s)

1300-2300

3000-7000

*Solvent: Butyl acetate

*Recommended Curing Agent: Covestro N3390

*Main Ratio: Calculated based on the actual hydroxyl value of the blended fluororesin

 

n Precautions:

  1. Store in a cool, dry, and well-ventilated place. Shelf life is 9 months; the product can still be used after the expiration date if it passes quality testing. 

      2. The product has an MSDS available upon request; please read it carefully before use.

 

 

 


Previous: 
Next: 

Changzhou Huake Polymer Co., Ltd.

Huake has always been devoted to providing customers with high-quality products and comprehensive solutions in the field of composite materials and adhesives through technological innovation.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-18648932615
 marketing@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap