HS-2119E
HUAKE
HS-2119E Unsaturated Polyester Resinae
Principal Properties & Application:
Orthophthalica fundata polyester resinsaturata media reactivitas, praeaccelerata, humilis viscositas, tempus gel selectabile, post curationem ieiunium, bonum fibra vitrea humida, altae proprietates mechanicae. Apta casula FRP operculo, turribus refrigerandis etc. magnis dimensionibus per RTM vel VARTM.
Specificationes liquidae resin
| Item | Unitas | Latin Requisita | Test Methodi | Item |
| Aspectus | Purpura rubrum vel lumen rubeum | GB/T 8237.6.1.1 | ||
| perspicuus liquor | ||||
| Viscositas (25℃) | cP | 120-160 | GB/T 7193.4.1 | |
| Gel Time(25℃) | min | 25.0-35.0 | GB/T 7193.4.6 | HS-2119E-G30H |
| 35.0-45.0 | HS-2119E-G40H | |||
| 45.0-55.0 | HS-2119E-G50H | |||
| 65.0-75.0 | HS-2119E-G70H | |||
| 95.0-115.0 | HS-2119E-G100H | |||
| 115.0-135.0 | HS-2119E-G120H | |||
| Acidum Pendo | mgKOH/g* | 17.0-25.0 | GB/T 2895 | |
| Firmus Content | % | 51.0-57.0 | GB/T 7193.4.3 |